Mechanical Properties Metric English Comments
Modulus of Rupture 0.0414 GPa
6.00 ksi
Abraded "A" Rods
Corning Vycor® 7930 Porous Glass
Open cell porous glass which exhibits excellent moisture absorbing properties ("thirsty"). It is mechanically hard and strong, nondusting, nonflaking, and chemically inert. These properties allow ..
Modulus of Rupture 0.0414 GPa
6.00 ksi
Blasch Ceramics NITRON Nitride bonded SiC
Features:Properties suit many severe operating conditionsGood wear and abrasionResists wetting by non-ferrous metalsHigh mechanical strengthExcellent Thermal shock resistance