Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0414 GPa | 6.00 ksi | Abraded "A" Rods |
Corning Vycor® 7930 Porous Glass Open cell porous glass which exhibits excellent moisture absorbing properties ("thirsty"). It is mechanically hard and strong, nondusting, nonflaking, and chemically inert. These properties allow .. |
|||
Modulus of Rupture | 0.0414 GPa | 6.00 ksi | |
Blasch Ceramics NITRON Nitride bonded SiC Features:Properties suit many severe operating conditionsGood wear and abrasionResists wetting by non-ferrous metalsHigh mechanical strengthExcellent Thermal shock resistance |