Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00600 GPa | 0.870 ksi | |
Pyrotek Pyrocast HD Castable Refractory Pyrocast HD is an insulating castable which is particularly suitable in applications where a combination of low thermal conductivity and long service life is required.ApplicationsLaunder lining Hot-.. |