Material Notes:
Pyrocast HD is an insulating castable which is particularly suitable in applications where a combination of low thermal conductivity and long service life is required.ApplicationsLaunder lining Hot-top table sections Header rings Sheet ingot tubes AdvantagesLow thermal conductivity Non-wetting Good thermal stability Easily machined Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
oven dried
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00600 GPa
0.870 ksi
Compressive Strength 13.0 MPa
1890 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.410 W/m-K

@Temperature 700 °C
2.85 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Maximum Service Temperature, Air 850 °C
1560 °F
Shrinkage -0.400 %

@Temperature 700 °C,
Time 10800 sec
-0.400 %

@Temperature 1290 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 48 %
48 %
CaO 30 %
30 %
Other 2.0 %
2.0 %
SiO2 20 %
20 %