Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.005886 - 0.007848 GPa @Temperature 1400 °C |
0.8537 - 1.138 ksi @Temperature 2550 °F |
|
Chosun Refractories CRAZ-L43 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 GPa @Temperature 1500 °C, Time 10800 sec |
0.8537 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories TAST-160 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 - 0.006867 GPa @Temperature 1400 °C |
0.8537 - 0.9960 ksi @Temperature 2550 °F |
|
Chosun Refractories CRAG-L42 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories TG-55 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |