Modulus of Rupture 0.005886 - 0.007848 GPa

@Temperature 1400 °C
0.8537 - 1.138 ksi

@Temperature 2550 °F
Chosun Refractories CRAZ-L43 Shroud Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 GPa

@Temperature 1500 °C,
Time 10800 sec
0.8537 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories TAST-160 Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 - 0.006867 GPa

@Temperature 1400 °C
0.8537 - 0.9960 ksi

@Temperature 2550 °F
Chosun Refractories CRAG-L42 Shroud Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories TG-55 Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).