Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00390 GPa | 0.566 ksi | parallel to thickness |
Zircar Refractory Composites RS-A2 Refractory Sheet This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee.. |