Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00390 GPa | 0.565 ksi | Dry Modulus of Rupture, 50% clay/50% flint, cast bars |
Old Hickory Volunteer Tennessee Ball Clay A versatile clay selection for casting, pressing, or plastic forming process methods. It is similar to M-23 in mineralogy with slightly more organic content. Volunteer has very good plasticity and i.. |
|||
Modulus of Rupture | 0.00390 GPa | 0.565 ksi | Green |
Unifrax Fibermax® Duraboard® 17H Board Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. .. |
|||
Modulus of Rupture | 0.00390 GPa | 0.566 ksi | parallel to thickness |
Zircar Refractory Composites RS-A2 Refractory Sheet This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee.. |