Mechanical Properties Metric English Comments
Modulus of Rupture 0.103 - 0.172 GPa

@Treatment Temp. 1260 °C,
Time 86400 sec
15.0 - 25.0 ksi

@Treatment Temp. 2300 °F,
Time 24.0 hour
Fired
Unifrax Foamfrax® RG Plus Insulation
Like Foamfrax RG, Foamfrax® RG Plus combines refractory ceramic fiber, refractory cement, and a high-temperature binder solution that can be combined in the field using the uniqued Foamfrax process..