Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.103 - 0.172 GPa @Treatment Temp. 1260 °C, Time 86400 sec |
15.0 - 25.0 ksi @Treatment Temp. 2300 °F, Time 24.0 hour |
Fired |
Unifrax Foamfrax® RG Plus Insulation Like Foamfrax RG, Foamfrax® RG Plus combines refractory ceramic fiber, refractory cement, and a high-temperature binder solution that can be combined in the field using the uniqued Foamfrax process.. |