Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00118 GPa @Treatment Temp. 1300 °C |
0.171 ksi @Treatment Temp. 2370 °F |
|
Sharadaa Ceramics REFINSUL ZAP-018 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Modulus of Rupture | 0.00118 GPa | 0.171 ksi | Dried at 110°C |
Sharadaa Ceramics REFINSUL ZAP-016 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |