Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.000700 GPa | 0.102 ksi | EN 993-6: 1995 |
Skamol Group Moler POROS Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Modulus of Rupture | 0.000700 GPa @Temperature 815 °C |
0.102 ksi @Temperature 1500 °F |
ASTM C268 |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |
|||
Modulus of Rupture | 0.000700 GPa @Temperature 1095 °C |
0.102 ksi @Temperature 2003 °F |
ASTM C268 |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |
|||
Modulus of Rupture | 0.000700 GPa @Temperature 540 °C |
0.102 ksi @Temperature 1000 °F |
Fired; ASTM C268 |
BNZ Materials Blazecrete 3000 G Dense Castable Blazecrete 3000 G is high alumina castable for service to 3000°F (1667°C). Used in building new and repairing old refractory linings, for gunningInformation provided by BNZ Materials Inc. |
|||
Modulus of Rupture | 0.000700 GPa @Temperature 815 °C |
0.102 ksi @Temperature 1500 °F |
ASTM C268 |
BNZ Materials Blazecrete 3000 G Dense Castable Blazecrete 3000 G is high alumina castable for service to 3000°F (1667°C). Used in building new and repairing old refractory linings, for gunningInformation provided by BNZ Materials Inc. |
|||
Modulus of Rupture | 0.000700 GPa | 0.102 ksi | ASTM C133 |
BNZ Materials BNZ-20 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Modulus of Rupture | 0.000700 GPa | 0.102 ksi | ASTM C133 |
BNZ Materials BNZ-23 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |