Mechanical Properties Metric English Comments
Modulus of Rupture 0.000700 GPa
0.102 ksi
EN 993-6: 1995
Skamol Group Moler POROS Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Modulus of Rupture 0.000700 GPa

@Temperature 815 °C
0.102 ksi

@Temperature 1500 °F
ASTM C268
BNZ Materials Blazecrete 2600 Dense Castable
Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as..
Modulus of Rupture 0.000700 GPa

@Temperature 1095 °C
0.102 ksi

@Temperature 2003 °F
ASTM C268
BNZ Materials Blazecrete 2600 Dense Castable
Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as..
Modulus of Rupture 0.000700 GPa

@Temperature 540 °C
0.102 ksi

@Temperature 1000 °F
Fired; ASTM C268
BNZ Materials Blazecrete 3000 G Dense Castable
Blazecrete 3000 G is high alumina castable for service to 3000°F (1667°C). Used in building new and repairing old refractory linings, for gunningInformation provided by BNZ Materials Inc.
Modulus of Rupture 0.000700 GPa

@Temperature 815 °C
0.102 ksi

@Temperature 1500 °F
ASTM C268
BNZ Materials Blazecrete 3000 G Dense Castable
Blazecrete 3000 G is high alumina castable for service to 3000°F (1667°C). Used in building new and repairing old refractory linings, for gunningInformation provided by BNZ Materials Inc.
Modulus of Rupture 0.000700 GPa
0.102 ksi
ASTM C133
BNZ Materials BNZ-20 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Modulus of Rupture 0.000700 GPa
0.102 ksi
ASTM C133
BNZ Materials BNZ-23 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..