Mechanical Properties Metric English Comments
Modulus of Rupture 0.000586 GPa
0.0850 ksi
Parallel to Thickness
Zircar Ceramics Z-MAG/2300 Soluble Fiber Insulation
ZIRCAR NON-RCF Insulation Type Z-MAG/2300 is a rigid combination of soluble NON-RCF silica magnesia glass fibers and inorganic binder. It is suitable for use as a substitute for insulation containin..