Modulus of Rupture <= 0.012753 GPa

@Temperature 1400 °C
<= 1.8497 ksi

@Temperature 2550 °F
Chosun Refractories CSN-A114 Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture <= 0.012753 GPa

@Temperature 1400 °C
<= 1.8497 ksi

@Temperature 2550 °F
Chosun Refractories CSN-A116 Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).