Mechanical Properties Metric English Comments
Modulus of Rupture 0.00362 GPa
0.525 ksi
Dry Modulus of Rupture, 50% clay/50% flint, cast bars
Old Hickory Taylor Blend Tennessee Ball Clay
A highly plastic clay suitable for a variety of extruded, pressed, or casting ceramic formulations. It is a fine PSD clay with low carbon content and excellent fired brightness.Information provided ..
Modulus of Rupture 0.00362 GPa
0.525 ksi
Dipped Joint; ASTM C198
BNZ Materials No. 2986 Mortar
No. 2986 is a highly refractory mortar very similar to Blakbond, but gray to tan in color. Temperature to 3000°F.Information provided by BNZ Materials Inc.