Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00183 GPa | 0.265 ksi | |
Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting Vacuum formed shapes are manufactured from high purity alumina silica fibers in one-piece design that eliminates metal leakage. No pre-heating required. Reusable, with proper treatment, for multip.. |