Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vacuum formed shapes are manufactured from high purity alumina silica fibers in one-piece design that eliminates metal leakage. No pre-heating required. Reusable, with proper treatment, for multiple casting campaigns.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.514 g/cc
0.0186 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00183 GPa
0.265 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 0.160 W/m-K

@Temperature 540 °C
1.11 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.240 W/m-K

@Temperature 815 °C
1.67 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Maximum Service Temperature, Air 1090 °C
1990 °F
Continuous
1260 °C
2300 °F
Shrinkage 0.330 %

@Temperature 400 °C
0.330 %

@Temperature 752 °F
0.330 %

@Temperature 730 °C
0.330 %

@Temperature 1350 °F