Mechanical Properties Metric English Comments
Modulus of Rupture 0.000790 GPa

@Treatment Temp. 815 °C
0.115 ksi

@Treatment Temp. 1500 °F
Pyrotek M-14 Compressible/Insulating Boards
ApplicationsSiphon gaskets Trough and ladle linings Tundishes Mill board substitute AdvantagesResistant to chemical attack Excellent thermal shock resistance Slightly flexible Moderately compressibl..
Modulus of Rupture 0.000790 GPa
0.115 ksi
ASTM C133
BNZ Materials BNZ-23A Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Modulus of Rupture 0.000790 GPa
0.115 ksi
BNZ Materials PA 23 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..