Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Modulus = 8400 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 57.9 GPa

@Temperature 21.1 °C
8400 ksi

@Temperature 70.0 °F
Wet; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Modulus 57.9 GPa

@Temperature 177 °C
8400 ksi

@Temperature 350 °F
Dry, 0° Direction; ASTM D6641
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Compressive Modulus 57.9 GPa

@Temperature 21.1 °C
8400 ksi

@Temperature 70.0 °F
Dry, 0° Direction; ASTM D6641
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Compressive Modulus 57.9 GPa

@Temperature 23.0 °C
8400 ksi

@Temperature 73.4 °F
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Fabric Form
Fiber: T300-3KInformation provided by HexCel
Compressive Modulus 57.9 GPa

@Temperature -59.0 °C
8400 ksi

@Temperature -74.2 °F
Dry
Hexcel® HexPly® F593 Epoxy Resin, F3T584 Carbon Fabric
Hexcel designation: F3T584-42"-F593; Fiber: Toray T-300/3kInformation provided by HexCel