Compressive Modulus 68.3 GPa

@Temperature 21.1 °C
9900 ksi

@Temperature 70.0 °F
Dry, 0° Direction; ASTM D695
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin T650-35-6K-UC309-5HS Carbon Fabric
Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures ..