Polymer Property : Compressive Modulus = 58.6 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 58.6 GPa

@Temperature 121 °C
8500 ksi

@Temperature 250 °F
Dry, 365° Oven Cured; SACMA 1R-94
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 12K PW HTS Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Compressive Modulus 58.6 GPa

@Temperature 82.2 °C
8500 ksi

@Temperature 180 °F
Wet; Autoclave Cured; SACMA 1-94
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Compressive Modulus 58.6 GPa

@Temperature 21.1 °C
8500 ksi

@Temperature 70.0 °F
Wet, 0° Direction; ASTM D6641
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Compressive Modulus 58.6 GPa

@Temperature 19.4 °C
8500 ksi

@Temperature 67.0 °F
CTD, 0° Direction; ASTM D6641
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Compressive Modulus 58.6 GPa

@Temperature 177 °C
8500 ksi

@Temperature 350 °F
Wet, 90° Direction; ASTM D6641
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Compressive Modulus 58.6 GPa

@Temperature 210 °C
8500 ksi

@Temperature 410 °F
Wet, 90° Direction; ASTM D6641
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Compressive Modulus 58.6 GPa

@Temperature 177 °C
8500 ksi

@Temperature 350 °F
Wet, 0° Direction; ASTM D6641
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Compressive Modulus 58.6 GPa

@Temperature 177 °C
8500 ksi

@Temperature 351 °F
T300, Plain Weave; Fill Compression; Wet
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Fabric Form
Fiber: T300-3KInformation provided by HexCel