Mechanical Properties Metric English Comments
Compressive Modulus 127 GPa

@Temperature 82.2 °C
18400 ksi

@Temperature 180 °F
Dry; Vacuum/Oven Cured; SACMA 1-94
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Compressive Modulus 127 GPa

@Temperature 121 °C
18400 ksi

@Temperature 250 °F
0°, Dry
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber
Information provided by HexCel