Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 127 GPa @Temperature 82.2 °C |
18400 ksi @Temperature 180 °F |
Dry; Vacuum/Oven Cured; SACMA 1-94 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Compressive Modulus | 127 GPa @Temperature 121 °C |
18400 ksi @Temperature 250 °F |
0°, Dry |
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber Information provided by HexCel |