Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 128 GPa @Temperature 25.0 °C |
18600 ksi @Temperature 77.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber Information provided by HexCel |