Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 76.5 GPa @Temperature 82.2 °C |
11100 ksi @Temperature 180 °F |
Wet; Autoclave Cured; SACMA 1-94 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 6K 4HS IM7 Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |