Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.00550 GPa

@Strain 5 %
0.798 ksi

@Strain 5 %
ISO-7743
Vicone High Performance Rubber VicoFluorâ„¢ 06FK-BR High Performance Fluoroelastomer Rubber
Meets ASTM D2000 fluoroelastomer 60 Durometer.