Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00550 GPa @Strain 5 % |
0.798 ksi @Strain 5 % |
ISO-7743 |
Vicone High Performance Rubber VicoFluorâ„¢ 06FK-BR High Performance Fluoroelastomer Rubber Meets ASTM D2000 fluoroelastomer 60 Durometer. |