Compressive Modulus 0.710 GPa

@Temperature 23.0 °C
103 ksi

@Temperature 73.4 °F
X direction, Condition A; ASTM D695
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate
RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to..
Compressive Modulus 0.710 GPa

@Temperature 23.0 °C
103 ksi

@Temperature 73.4 °F
Y direction, Condition A; ASTM D695
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate
RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to..