Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00280 GPa @Strain 5 % |
0.406 ksi @Strain 5 % |
ISO-7743 |
Vicone High Performance Rubber VicoSilâ„¢ 159DLK-RD High Performance Silicone Rubber Meets AMS 3302 Silicone 50 Durometer. |