Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.000790 GPa @Strain 10.0 % |
0.115 ksi @Strain 10.0 % |
|
Vicone High Performance Rubber VicoSealâ„¢ 106C-BK High Performance EPDM Rubber Information provided by Vicone |