Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Vicone High Performance Rubber VicoSeal™ 106C-BK High Performance EPDM Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Vicone High Performance Rubber
Trade Name VicoSeal™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vicone High Performance Rubber VicoSeal™ 106C-BK High Performance EPDM Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Vicone
Physical Properties Metric English Comments
Density 1.497 g/cc
0.05408 lb/in³
ASTM D3165
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
68.04

@Treatment Temp. 100 °C,
Time 252000 sec
68.04

@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D412
11.74 MPa

@Treatment Temp. 100 °C,
Time 252000 sec
1703 psi

@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Elongation at Break 540.8 %
540.8 %
ASTM D412
430.48 %

@Treatment Temp. 100 °C,
Time 252000 sec
430.48 %

@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Compressive Modulus 0.000540 GPa

@Strain 5.00 %
0.0783 ksi

@Strain 5.00 %
0.000790 GPa

@Strain 10.0 %
0.115 ksi

@Strain 10.0 %
0.00153 GPa

@Strain 20.0 %
0.222 ksi

@Strain 20.0 %
0.00196 GPa

@Strain 25.0 %
0.284 ksi

@Strain 25.0 %
Compression Set 6.49 %

@Temperature 100 °C,
Time 79200 sec
6.49 %

@Temperature 212 °F,
Time 22.0 hour
ASTM D395
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved