Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.000750 GPa @Strain 25.0 % |
0.109 ksi @Strain 25.0 % |
|
Vicone High Performance Rubber VicoSilâ„¢ C303Q-GY High Performance Silicone Rubber Information provided by Vicone |