Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Vicone High Performance Rubber
Trade Name VicoSil™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vicone High Performance Rubber VicoSil™ C303Q-GY High Performance Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Vicone
Physical Properties Metric English Comments
Density 1.134 g/cc
0.04097 lb/in³
ASTM D3165
Mechanical Properties Metric English Comments
Hardness, Shore D 32
32
ASTM D2240
30.4

@Treatment Temp. 200 °C,
Time 252000 sec
30.4

@Treatment Temp. 392 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Tensile Strength, Yield 6.50 MPa
943 psi
ASTM D412
3.8155 MPa

@Treatment Temp. 200 °C,
Time 252000 sec
553.39 psi

@Treatment Temp. 392 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Elongation at Break 709.2 %
709.2 %
ASTM D412
539.7 %

@Treatment Temp. 200 °C,
Time 252000 sec
539.7 %

@Treatment Temp. 392 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Compressive Modulus 0.000200 GPa

@Strain 5.00 %
0.0290 ksi

@Strain 5.00 %
0.000320 GPa

@Strain 10.0 %
0.0464 ksi

@Strain 10.0 %
0.000410 GPa

@Strain 20.0 %
0.0595 ksi

@Strain 20.0 %
0.000750 GPa

@Strain 25.0 %
0.109 ksi

@Strain 25.0 %
Compression Set 6.31 %

@Temperature 175 °C,
Time 79200 sec
6.31 %

@Temperature 347 °F,
Time 22.0 hour
ASTM D395
Descriptive Properties Value Comments
Color Cool Gray