Mechanical Properties Metric English Comments
Compressive Modulus 0.00500 GPa

@Strain 20 %
0.725 ksi

@Strain 20 %
ISO-7743
Vicone High Performance Rubber VicoSilâ„¢ 369DLK-GY High Performance Silicone Rubber
UL94 approved