Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00450 GPa @Strain 5 % |
0.653 ksi @Strain 5 % |
ISO-7743 |
Vicone High Performance Rubber VicoSilâ„¢ 369DLK-GY High Performance Silicone Rubber UL94 approved |