Polymer Property : Compressive Strength = 9200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 63.4 MPa

@Temperature 1667 °C
9200 psi

@Temperature 3033 °F
Cold Crush Strength; At Use Limit
BNZ Materials Blazecrete 3000 Dense Castable
Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec..