Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 53.8 MPa @Temperature 1778 °C |
7800 psi @Temperature 3232 °F |
Cold Crush Strength; At Use Limit |
BNZ Materials Blazecrete 3200 Dense Castable Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special .. |