Mechanical Properties Metric English Comments
Compressive Strength 53.8 MPa

@Temperature 1778 °C
7800 psi

@Temperature 3232 °F
Cold Crush Strength; At Use Limit
BNZ Materials Blazecrete 3200 Dense Castable
Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special ..