Mechanical Properties Metric English Comments
Compressive Strength 43.0 MPa

@Strain 17.6 %,
Temperature 100 °C
6240 psi

@Strain 17.6 %,
Temperature 212 °F
Z direction, Condition A; ASTM D695
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate
RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to..
Compressive Strength 43.0 MPa

@Strain 1 %
6240 psi

@Strain 1 %
ISO 604
Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data)
Compared with virgin PA 66, this 30 % glass fibre reinforced and heat stabilised nylon grade offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining an exce..