Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 6090 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 42.0 MPa

@Strain 1 %
6090 psi

@Strain 1 %
ISO 604
Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data)
Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors fo..
Compressive Strength 42.0 MPa

@Temperature 815 °C
6090 psi

@Temperature 1500 °F
Cold Crush Strength
BNZ Materials Blazecrete 3200 Dense Castable
Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special ..
Copyright © lookpolymers.com All Rights Reserved