Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 41.2 MPa @Temperature 110 °C, Time 86400 sec |
5970 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories CTL ASP-RF Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 41.2 MPa @Temperature 1000 °C, Time 10800 sec |
5970 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories SFC-70R High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |