Mechanical Properties Metric English Comments
Compressive Strength 41.2 MPa

@Temperature 110 °C,
Time 86400 sec
5970 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories CTL ASP-RF Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 41.2 MPa

@Temperature 1000 °C,
Time 10800 sec
5970 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SFC-70R High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).