Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 48.0 MPa @Strain 2 % |
6960 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Nylatron® 703XL PA 6 + internal lubricant, cast (ISO Data) This high performance cast nylon 6 bearing grade provides an even better wear resistance than Nylatron NSM, combined with good pressure-velocity capabilities and a near zero level of “stick-slip”... |