Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 29.6 MPa @Treatment Temp. 540 °C |
4290 psi @Treatment Temp. 1000 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Blazecrete 3000 Dense Castable Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec.. |
|||
Compressive Strength | 29.6 MPa @Temperature 1095 °C |
4290 psi @Temperature 2003 °F |
Cold Crush Strength |
BNZ Materials Blazecrete 3200 Dense Castable Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special .. |