Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 37.7 MPa @Temperature 1100 °C, Time 10800 sec |
5460 psi @Temperature 2010 °F, Time 3.00 hour |
Cold Crushing, Typical Value, After firing @ 1100°C |
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd. |