Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 360 MPa @Temperature 23.0 °C |
52200 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |