Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 219 MPa @Temperature 150 °C |
31800 psi @Temperature 302 °F |
ISO 604 |
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri.. |