Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 170 - 190 MPa @Temperature 1200 °C |
24700 - 27600 psi @Temperature 2190 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values .. |