Mechanical Properties Metric English Comments
Compressive Strength 17.9 MPa

@Temperature 1260 °C
2600 psi

@Temperature 2300 °F
Cold Crush Strength
BNZ Materials Blazecrete 2300 ARG Dense Castable
Blazecrete 2300 ARG is an alumina-silica castable with high strength and abrasion resistance. For service to 2300°F (1260°C). May be gunned or slap-troweled over Blaz 2000G to obtain a high streng..